Wednesday, 6 July 2011

Time to actually get the epoxy out

In order to join each pair of panels I had decided to make a scarf joint 40mm long.  The recommended length I think is 60mm, but when I was practising on some scrap I found I could not get an even wedge shape over that great a distance, so 40mm was all I could manage.

The process is to clamp - and I also used panel pins - two panels on top of each other - but the top one is set back by 40mm.  Then set to with the belt sander.  Keep watch on the different coloured lines as they appear, try and keep them even on both panels.  Keep going until you have got an even wedge which goes 40mm back on both panels.

This took plenty of practice - and even then some were not too clever - this is one of the better ones

I was not too bothered, as the thickened epoxy will fill any imperfections, voids in the plywood which become apparent.

Then to make sure the scarf joints were glued correctly, both in the sense of the correct over lap, and that they need to exactly join so the plank has the correct, and matching curves, I did a lot measuring and marking on my bench.  I marked the 305mm spacing lines that were used for original points plotting onto the edges of all the sheets.  Then I marked on the bench the exact point (left and right of the centre point where the scarf joint is) of the 5th station, so when I laid a pair of panels end to end for glueing I could make sure that the centre, and the 5th station points were correct and I knew the final panel would be absolutely correct.
Finally, with layers of dustbin liner between I glued the panels together in pairs.  I used panel pins to nail then to a wood block, to hold them steady, put another block on top and clamped them together.
So I had five set of 4 metre panels with assorted clamps and blocks lying, curing on the floor.  So I thought.....

Sorry no pictures here I was to sticky and tired, and forgot.

You remember that discussion about using clear plastic pots to mix the epoxy, well, I decided to splash out and buy some pumps.  These are already set to give epoxy and hardner in the ratio of 5 : 1  (one pump on each gives the right ratio)  BUT I thought ( without reading the instructions ) 5 : 1 means 5 pumps and 1 pump.  I duly did this, added my wood filler, and silica, spread, nailed clamped etc.  Next day I cam back - and surprise NOT cured!   ( What an error for a Maths teacher)
After much scraping, and remixing, and renailing and re clamping I finally had 10 long sheets of plywood.

That lot took another day of about 8 hours, and about 2 hours the next day re-glueing.